Gas carburising is the most widely used method of chemical heat treatment of steel. The surface of the part is enriched with carbon and, after quenching, gains a hard, wear-resistant case — while the core stays tough. It is used mainly for loaded machine parts such as gears, shafts and pins.
Gas carburising, Poland. Arranged at a vetted plant in Poland, to order, with a non-binding enquiry.
We do not carry out carburising ourselves. reliq is your first point of contact — send us an enquiry and we will connect you with a proven plant in Poland, help you choose the technology and handle communication. You then sign the order, contract and warranty directly with the plant.
Carburising is a thermochemical diffusion process that enriches the surface of low-carbon steel (typically around 0.25% carbon) with carbon. The carbon diffuses into the surface layer, which transforms into hard martensite after quenching, while the core stays tough. The goal is high surface hardness and wear resistance combined with a tough core.
The effective case depth (ECD) can range from shallow cases, often below 2 mm, up to deep cases of 4–6 mm. It is defined as CHD to EN ISO 2639 (the point with a hardness of 550 HV1). Surface hardness is typically around 58–62 HRC.
Carburising is ideal where a part needs a hard, wear-resistant surface together with a tough core that resists impact and fatigue, often even with deeper cases.
Suitable steels are low-carbon alloy case-hardening steels such as 16MnCr5, 20MnCr5 or 18CrNiMo7-6.
| Process | Element | Temperature | Typical use |
|---|---|---|---|
| Carburising | carbon | 880–980 °C | larger parts, deeper cases |
| Carbonitriding | carbon + nitrogen | 820–900 °C | smaller parts, less distortion |
| Nitriding | nitrogen | ~520 °C | thin, very hard case, no quench |
See also carbonitriding, nitriding and vacuum carburising (LPC).
After carburising and quenching the surface typically reaches 58–62 HRC, while the core stays tough.
Effective case depth (ECD) ranges from shallow cases (often below 2 mm) up to 4–6 mm. It is defined as CHD to EN ISO 2639 (hardness 550 HV1).
Low-carbon alloy case-hardening steels such as 16MnCr5, 20MnCr5 or 18CrNiMo7-6.
No. reliq is an agent: we connect you with a proven plant in Poland and help you choose the technology and handle communication. You sign the order and warranty directly with the plant.
Send us a non-binding enquiry. We will connect you with a proven plant in Poland and help you choose the technology and parameters.
Send an enquiry →