Home  /  Heat treatment  /  Carbonitriding

Carbonitriding

Carbonitriding is an austenitic process in a carburising furnace, similar to carburising but with added nitrogen. It forms a harder case than carburising and, thanks to the lower temperature and milder quench, has less distortion — ideal for smaller, more delicate parts and clean high-volume production.

Carbonitriding, Poland. Arranged at a vetted plant in Poland, to order, with a non-binding enquiry.

We do not carry out carbonitriding ourselves. reliq is your first point of contact — send us an enquiry and we will connect you with a proven plant in Poland, help you choose the technology and handle communication. You then sign the order, contract and warranty directly with the plant.

Environment
Carburising furnace
Temperature
820–900 °C
Benefit
Harder case, less distortion
Terminology: carbonitriding is an austenitic process in a carburising furnace with quenching. Do not confuse it with nitrocarburising, which runs in the ferritic range in a nitriding furnace without quenching.
Step 1
C + N enrichment
In the austenitic range (820–900 °C) the surface is enriched with both carbon and nitrogen.
Step 2
Oil quench
Nitrogen allows a milder quench → less distortion and lower cracking risk.
Step 3
Tempering
Low-temperature tempering stabilises the structure.

What is carbonitriding

Carbonitriding is an austenitic process similar to carburising, with added nitrogen. Nitrogen increases the hardenability of the case, stabilises austenite and lowers the critical quench rate — so a milder oil quench can be used, with less distortion, and a case even harder than plain carburising is formed. The surface takes up roughly 0.5–0.8% carbon and 0.2–0.4% nitrogen.

Case depth

The case depth (CHD) usually does not exceed about 0.75 mm (typically 0.1–0.75 mm) and depends on the quench temperature, cooling rate, steel hardenability and part size.

When to choose carbonitriding

Carbonitriding is excellent for clean, high-volume production of smaller parts that need high wear resistance together with limited distortion.

Carbonitriding vs. carburising

AspectCarbonitridingCarburising
Elementscarbon + nitrogencarbon
Temperature820–900 °C880–980 °C
Case depththinner (0.1–0.75 mm)deeper (up to 4–6 mm)
Distortionlowerhigher

For larger parts and deeper cases, gas carburising is more suitable. For low-temperature treatment without quenching see nitrocarburising or nitriding.

FAQ

What is the difference between carbonitriding and nitrocarburising?

Carbonitriding is austenitic, runs in a carburising furnace at 820–900 °C and is followed by quenching; carbon dominates. Nitrocarburising is ferritic, runs in a nitriding furnace without quenching; nitrogen dominates.

What is the case depth?

Usually up to about 0.75 mm (typically 0.1–0.75 mm), i.e. less than carburising.

Why does carbonitriding cause less distortion?

It runs at a lower temperature than carburising and nitrogen allows a milder oil quench.

Does reliq carry out carbonitriding itself?

No. reliq is an agent: we connect you with a proven plant in Poland and help you choose the technology and handle communication. You sign the order and warranty directly with the plant.

Need parts carbonitrided?

Send us a non-binding enquiry. We will connect you with a proven plant in Poland and help you choose the technology and parameters.

Send an enquiry →

← Back to heat treatment