A complete overview of processes available at vetted partners.
An indicative overview of available heat- and thermochemical-treatment technologies — principle, environment, temperatures, suitable materials and typical real-world applications. Specific parameters are always confirmed by the vetted partner according to your part and material.
| Process | Principle | Atmosphere / environment | Temperature | Suitable materials | Typical applications (segment · parts) |
|---|---|---|---|---|---|
| Hardening (oil / gas) | Austenitizing and rapid cooling → hard martensitic structure. | Protective (endogas, N₂) or oil bath | 820–1050 °C | Uhlíkové a legované oceli (> 0,3 % C), nástrojové oceli | Automotive, heavy industry · gears, shafts, connecting rods, pins |
| Vacuum hardening | Austenitizing in vacuum, gas-pressure quench (N₂/He) → clean bright surface, low distortion. | Vacuum + gas quench | 1000–1250 °C | Tool and high-speed steels, martensitic stainless steels | Tool shops, aerospace, medical · punches, cutting dies, molds, stainless parts |
| Tempering | Heating quenched steel below Ac₁ → stress relief, increased toughness. | Protective / air | 150–650 °C | Quenched steels | All sectors · parts after hardening (hardness and stress stabilization) |
| Annealing (normalizing, soft, stress-relief) | Heating and controlled slow cooling → structure adjustment, softening, removal of internal stress. | Protective | 550–950 °C | Steels, cast irons | Engineering, heavy industry · forgings, semi-finished products, large cross-sections |
| Isothermal annealing | Austenitizing, cooling to the pearlite-transformation temperature and holding → uniform, easily machinable structure. | Protective | 850–950 °C → výdrž 600–700 °C | Case-hardening and alloy steels | Automotive, tool shops · gear blanks and tool steels |
| Solution annealing | Heating to dissolve precipitates and rapid cooling → homogeneous solid solution. | Vacuum / protective | 1000–1150 °C | Austenitic and PH stainless steels, Ni/Co superalloys | Aerospace, medical · stainless and superalloy parts, flanges, heat exchangers |
| Precipitation hardening (aging) | After solution annealing, controlled heating → precipitation of strengthening phases and increased strength. | Vacuum / protective | 480–760 °C | Precipitation-hardening (PH) stainless 17-4 PH, Ni superalloys (IN718) | Aerospace, tool shops · PH stainless and superalloys, molds, engine parts |
| Vacuum brazing | Joining parts with molten filler in vacuum without flux → clean, strong joints. | Vacuum | 800–1200 °C | Stainless steel, Ni/Co superalloys, steels | Aerospace, medical · heat exchangers, stainless assemblies |
| Process | Principle | Atmosphere / environment | Temperature | Suitable materials | Typical applications (segment · parts) |
|---|---|---|---|---|---|
| Carburizing (gas) + quench | Carbon diffusion into the surface followed by quenching → hard surface, tough core. | Endogas + hydrocarbon | 880–950 °C | Case-hardening steels (16MnCr5, 18CrNiMo7-6) | Automotive, heavy industry · gears, shafts, differential cases |
| Vacuum carburizing (LPC) | Carburizing in vacuum with acetylene, gas-pressure quench → clean surface without internal oxidation. | Low-pressure vacuum (C₂H₂) | 900–1050 °C | Case-hardening steels, complex-shaped and precision parts | Automotive, aerospace · precision gears, transmission shafts |
| Carbonitriding | Simultaneous carbon and nitrogen enrichment followed by quenching → hard surface at lower temperature and less distortion. | Endogas + hydrocarbon + NH₃ | 780–880 °C | Low-carbon and low-alloy steels, sheet-metal parts | Automotive · pressed and sheet-metal parts, small gears |
| Nitriding (gas) | Nitrogen enrichment of the surface below Ac₁ without phase transformation → high hardness, minimal distortion. | NH₃ (gas) | 500–580 °C | Nitriding steels (31CrMoV9, 34CrAlNi7-10), alloy steels | Automotive · camshafts, precision parts (min. distortion) |
| FNC – ferritic nitrocarburizing | Nitrogen and carbon enrichment in ferrite without quenching → thin hard compound layer (ε), resistance to wear and galling. | NH₃ + endogas / salt bath / plasma | 560–590 °C | Unalloyed and alloy steels, cast iron | Automotive, series production · connecting rods, brake and hydraulic parts |
| Post-oxidation | After nitriding / FNC, controlled surface oxidation → black oxide layer (Fe₃O₄), higher corrosion resistance and appearance. | Oxidizing (steam / controlled air) | 350–550 °C | Steels after nitriding / FNC | Automotive · parts requiring corrosion resistance and appearance |
Applying functional coatings from molten material at high velocity — protection against wear, corrosion and high temperatures. The substrate remains practically thermally unaffected; coatings based on carbides (WC-Co), ceramics or metals. Suitable for parts in automotive, aerospace and power generation.